I'd already experienced this issue, when printing with salt water, but with a major difference. I use FunToDo resin, which needs many hours to the pigments to go down. The snow white resin "loose" pgmentation faster than lack or red ftd resin. Nevertheless, I successfully print object that takes around 10hrs, without any problem. The pigments form a 3rd layer, only the day after. For red resins, I think this takes more time.Statistics: Posted by FR3Dprint — Fri Nov 27, 2015 8:28 am
]]>